Wear Parts & Structural Items
Wear liners, discharge chutes, gates, door seals, rubber pads, structural steel, bolts and fasteners.
Wear & Structural Parts for Concrete Batching Plants
Quality replacement parts with factory-direct pricing. Contact us for a complete list.
Available Wear & Structural Parts
| Part Name | Common Material | Specifications |
|---|---|---|
| Wear Liners | NM400 / NM500 steel | Custom shapes |
| Chute Liners | Ceramic / rubber composite | For transfer points |
| Baffle Plates | High-chromium alloy | For mixers |
| Scraper Blades | Hardened alloy steel | For belt conveyors |
| Structural Steel | Q235 / Q345 | Custom fabrication |
How to Order the Right Parts
To ensure the correct fit, please provide us with:
- Your mixer / plant model (e.g. HZS120, JS2000)
- The part name and quantity needed
- Photos or drawings of the worn part (if available)
- Your plant's serial number or year of manufacture
Need a quote? Send us your plant model and part list — we respond within 4 hours with specifications, material options and factory pricing. WhatsApp: +86 187 6888 8850
Wear & Structural Parts FAQ
What material do you recommend for wear liners?
For high impact use NM400/NM500; for abrasive sliding use ceramic composite liners. We advise based on your application.
Can you fabricate custom wear parts?
Yes, send us drawings or samples and we will fabricate exact replacements in the required steel grade.
Do you supply chute liners for transfer points?
Yes, ceramic and rubber composite liners for chutes and transfer points, custom cut to size.
How do I know when the liner plates need replacing?
When the plate has worn down to the point that the bolt heads are exposed or nearly so, or the shell behind it starts to show wear marks. Measuring thickness at three points — inlet, middle, discharge — tells you whether wear is uniform or localised.
Why are my mixing blades wearing on one side only?
Usually shaft alignment or one-sided aggregate loading. Check that the shaft is true and that material is not consistently entering the trough at one end. Also check the arm torque — a loose arm lets the blade angle change under load.
What should the blade-to-liner clearance be?
Set it to the figure for your mixer model when new liners go in, then re-check after a month as the plates settle. If you do not have the figure, set the clearance as small as the trough allows without contact through a full revolution, and verify by hand before running loaded.
Can liners be replaced without removing the shaft?
On most twin-shaft mixers yes, working through the inspection doors, but it is slow and awkward. If several plates need changing at once, pulling the shaft is usually faster overall and lets you inspect the arms and bearings at the same time.
Read the wear pattern before you order
Liner plates and mixing blades are the parts customers reorder most often, and the wear pattern on the old set tells you more than any catalogue. Uniform wear across the trough is normal consumption. Wear concentrated in one band, or on one side of the shaft, is a symptom of something that will eat the new set just as fast.
Wear concentrated at the discharge end usually means the batch is being mixed too dry at the start or the discharge gate is being opened early, so material grinds against the same area every cycle. Wear on one side only points at shaft alignment, or at aggregate being loaded consistently into the same end of the trough. Blades that are worn on the leading edge but sharp on the trailing edge are working; blades worn thin across the full face are being run with too large a clearance and are pushing material rather than folding it.
Wear part replacement triggers
| Part | Replace when | Consequence of waiting |
|---|---|---|
| Trough liner plates | Worn through to the bolt heads, or plate thickness down by roughly half | Trough shell starts wearing — a fabrication job instead of a bolt-on |
| Mixing blades / arms | Leading edge rounded back, or blade-to-liner clearance visibly open | Poor mix uniformity, longer cycle times, higher power draw |
| Discharge gate seal | Material weeping at the gate when closed | Segregation, dust, and wear on the gate face |
| Bin gate and gate rubber | Torn rubber or gate not seating | Aggregate leakage and weigh hopper errors |
| Dust sleeve / rubber boot | Cracks or holes at the flex point | Dust at the mixer platform and material loss |
| Skip wheels and track | Flat spots, or skip running uneven | Track damage and shock loading on the frame |
Blade clearance decides liner life
The gap between the blade tip and the liner is the number that quietly controls how fast you buy both. Too large and a wedge of material sits under the blade, grinding the liner and leaving unmixed sand against the shell. Too small and the blade contacts the liner on the first slightly oval trough or worn bearing. Check the clearance after fitting new liners, and check it again after a month, because new plates settle onto the bolt pattern.
Replace liners and blades as a set where the budget allows. A new blade against a worn liner starts with a large clearance and will wear faster than either part did before.